1. To remove a molding closing a place of a leak. In certain cases dismantle of additional details can be demanded to localize a leak place. |
2. To note not tight place. Carefully to press from within glass, to specify extent of defect of consolidation. At this time glass should pour down outside water. To note extent of the damaged place. |
3. To wash out water a zone adjacent to not tight place, from dirt and extraneous substances. Then to dry a current of air. |
4. By means of a sharp knife to remove from a defective place pressurizing structure on length of 75-100 mm (from both parties). |
5. To put on the damaged place a priming coat, using materials from a repair set. Before use it is necessary to mix packing contents. To dry within 5 minutes. |
6. To put from two parties pressurizing structure on the damaged place (on length of 75-100 mm). |
7. At once after drawing to distribute and press pressurizing structure into cracks between glass and a frame of a window aperture for ensuring tightness of connection. To use for this purpose a flat shovel or other suitable tool. |
8. By means of a stream of warm or hot water to check tightness of consolidation. It is not necessary to direct a strong stream of water on svezhenanesenny pressurizing structure. |
9. To establish into place everything previously the dismantled details. |